Industrial Coatings Manufacturer & Global Flooring Solutions Contractor
KAIDA PAINT® · Manufacturer & Installer
What we supply
| Family | Build | Declared ceiling | Specify it for | Detail |
|---|---|---|---|---|
| Vinyl ester | 2–5 mm laminate 5–20 mm mortar | 75% sulfuric acid as a laminate; 95% as a mortar; 55% HF as mortar | Bunded areas, tank farms, plating lines, sumps, immersion duty | Vinyl ester systems |
| Epoxy mortar | 2–10 mm | 65% sulfuric acid; good on alkali | Load-bearing floors with moderate acid, where impact matters more than immersion | Epoxy mortar |
| Polyester FRP | 2–5 mm | 75% sulfuric acid, quoted 3–5 years | Medium duty where the budget sets the ceiling and replacement is planned | FRP flooring |
| Ceramic brick | Brick lining on bedding | 99.8% acid resistance, 0.2% water absorption, −20 to +130 °C | Hot concentrated acid, abrasion, impact; the step above every resin | Acid-resistant brick |



| Medium | Family | Declared ceiling | Above that |
|---|---|---|---|
| Sulfuric acid | Vinyl ester | 75% laminate; 95% mortar | Ceramic brick; oleum moves to carbon brick |
| Hydrochloric acid | Vinyl ester | 35–40% | Ceramic brick |
| Hydrofluoric acid | Vinyl ester mortar | 55% mortar; 25% in glass-reinforced coating | Carbon brick or PTFE — HF attacks silica in ceramic |
| Phosphoric acid | Vinyl ester | 80% | Ceramic brick |
| Sodium hypochlorite | Vinyl ester | No published ceiling immersion test | Not specified without a test |
| Solvents (aromatic, ketone, chlorinated) | None by default | Immersion test required | Lining, not a floor |








Volume is agreed against the system and the colour rather than as one blanket figure, because a 20 mm mortar and a 3 mm coating consume very different quantities per square metre. Send the area and the medium and we will quote at that size.
7–14 days for standard systems held in stock, against the 30 days typical of made-to-order supply. 3,000+ tonnes is held at the plant for that reason.
Yes. Crews are mobilised from the plant for turnkey work, or we supervise your contractor, or we train your team and sign off the first project. All three models have been used on overseas projects, including Sweden, Hungary, Venezuela and Rwanda.
Yes. A trial batch in the exact colour and system is sent before the first production run, so adhesion and cure are tested on your substrate rather than ours.
Film thickness and pull-off adhesion results, batch records, and the system specification as built. That pack is what an auditor or a client’s engineer asks for later.
We will say it. Above 55% hydrofluoric acid, or continuous solvent immersion, the answer is a different class of lining and we will tell you that instead of quoting a system that fails.
Contact: Ms. Sabella Wei
Phone: 86-022-83859963