Описание
Heavy duty anti static flooring is a resin floor built to carry loads that would crack a standard 3 mm coating — forklifts, steel-wheeled trolleys, dropped billets — while still providing a controlled path to earth for static charge. ACF-HX-SM-AS-SL is built at 8–12 mm and declared against 75% sulfuric acid and 40% hydrochloric acid. The ACF-HX-SM-AS-SL system embeds a welded steel mesh in an epoxy mortar body, levels with glass flake mortar, and finishes with a vinyl ester self leveling topcoat at 8–12 mm total thickness. This page explains how the mesh changes the load behavior, what the finished system resists, and where the extra thickness is genuinely necessary rather than simply reassuring.
| Артикул | Технические характеристики |
|---|---|
| Система | Steel mesh reinforced heavy duty anti static self leveling flooring |
| Model | ACF-HX-SM-AS-SL |
| Body | Epoxy penetrating primer, epoxy mortar with welded steel mesh, glass flake epoxy mortar leveling |
| Finish | Vinyl ester anti static self leveling topcoat |
| grounding (earthing) | Copper foil tapes connected to the building earth |
| Finished thickness | 8–12 mm (0.31–0.47 in) |
| Service life quoted | 15+ years in the duty it was specified for |
| Application method | Trowel-applied mortar and mesh, poured topcoat, ambient cure |
Why does heavy duty anti static flooring need steel mesh?
Resin mortar is strong in compression and weak in tension. Put a 3-tonne forklift on a 3 mm coating and the slab beneath deflects; the coating cracks because it has nothing to carry the tensile strain. Steel mesh embedded in the mortar body changes that: the mesh carries tension, spreads point loads over a wider area, and keeps cracks closed if the slab does move.
Three site conditions make the mesh version the right answer rather than an upsell:
- Point loads from small wheels. A pallet truck wheel imposes more stress per square centimetre than a car tire. Without reinforcement, the mortar crushes under the wheel path.
- Thermal movement in large slabs. A floor poured in bays moves; the mesh distributes that movement so the surface does not open at one line.
- Impact and abrasion together. Battery and plating plants drop jigs; mineral and steel plants drag loads. Thickness alone resists abrasion, but it is the mesh that stops impact from propagating a crack.
At 8–12 mm, the system can be repaired by cutting back and rebuilding a patch, rather than a coating that has to be stripped when it fails.
For chemical duty without an ESD requirement, see vinyl ester flooring.
What does the finished system resist?
The chemical envelope here is set by the vinyl ester topcoat and the glass flake mortar beneath it. The values below apply to the finished system, tested by 7-day immersion.
| Средний | Concentration | Результат |
|---|---|---|
| Sulfuric acid | 75% | No change after 7 days |
| Hydrochloric acid | 40% | No change after 7 days |
| Nitric acid | 45% | No change after 7 days |
| Acetic acid | 60% | No change after 7 days |
| Sodium hydroxide | 80% | No change after 7 days |
| Hydrofluoric acid | 20% | No change after 7 days |
| Phosphoric acid | 90% | No change after 7 days |
Note the alkali figure: 80% sodium hydroxide is a strong caustic load, and it is stated separately from the acid results because caustic attack is a different mechanism. Buyers often check only acid resistance and then discover the floor is washed with hot caustic.
For thin-film ESD without steel mesh, see anti static vinyl ester flooring.
Does the steel mesh interfere with the grounding path?
The mesh is structural, the grounding is electrical, and both occupy the same build, so the interaction has to be designed rather than assumed.
Steel mesh is a conductor. Laid as a continuous sheet across the floor, it forms an equipotential plane of its own unless it is bonded to the grounding system. Left unbonded, it can hold a charge separately from the conductive network and distort the reading a surface-resistance test is trying to take.
Three rules settle it in practice. The mesh is bonded to the grounding grid at defined points, so the whole floor sits at one potential instead of two. The conductive network — copper foil or conductive putty — is kept at a defined separation so the test current has a predictable path. And mesh continuity is checked before the topcoat goes down, because a mesh cut to clear a plinth no longer forms the plane it was specified to form.
Ask for the grounding layout and the mesh-bonding detail on one drawing. When they arrive as two drawings, the two systems have not been designed together.
Load and chemistry rarely arrive separately, so the comparison by duty is in corrosion resistant flooring under wheel load.
How is the build assembled?

- Concrete substrate — ground, sound, and structurally repaired where required.
- Epoxy penetrating primer — anchors the system into the slab.
- Epoxy mortar with welded steel mesh — the load-carrying layer; the mesh is laid in the wet mortar with the specified lap and cover.
- Grinding and leveling — the mortar is ground to plane before the next layer.
- Glass flake epoxy mortar — leveling and additional barrier thickness; glass flake platelets lengthen the diffusion path for water and chemicals.
- Conductive putty and copper foil grid — the charge-spreading layer and the earth path, with continuity checked before the topcoat.
- Vinyl ester anti static self leveling topcoat — the chemical barrier and the wearing surface.
The mesh is not decorative. Its lap width, cover depth and position within the mortar are specified, because a mesh laid too close to the surface becomes a corrosion site and a mesh laid too deep does not carry tension where it is needed.
What are the mechanical properties?
| Test item | Unit | Результат |
|---|---|---|
| Прочность на сжатие | N/mm² | ≥ 60 (8,700 psi) |
| Pencil hardness | H | ≥ 2H |
| Abrasion loss (750 g / 500 r) | g | ≤ 0.02 |
| Устойчивость к ударам | Kg/cm² | ≥ 80 |
Read these together with the thickness: the same compressive strength at 8–12 mm performs very differently from the same value at 3 mm, because load spreading depends on depth. That is why the quoted service life here is 15+ years rather than the 5–8+ years of the thin-film systems.
Where is heavy duty anti static flooring specified?
- Electroplating, anodising and surface treatment plants with forklift and jig traffic
- PCB and circuit board factories, where acid drag-out meets pallet handling
- Battery plants — formation, assembly and electrolyte handling areas
- Heavy industrial halls, steel fabrication and machinery assembly
- Power plant control rooms and switch rooms, where ESD control and floor durability meet
- Mineral processing and materials handling areas with abrasive spillage

Where load is moderate and thickness is the cheaper lever, see high build mortar flooring.
How is heavy duty anti static flooring installed?
- Подготовка — grinding, structural repair, moisture and dew-point check.
- Грунтовка — epoxy penetrating primer.
- Mesh and mortar — steel mesh laid to the specified grid, epoxy mortar trowelled in and around it.
- Grinding — mortar ground to plane and to the specified thickness.
- Glass flake mortar — leveling layer applied and ground.
- Conductive putty and copper grid — applied and continuity verified.
- Vinyl ester topcoat — poured and spread to the specified thickness; satin or anti-slip grades available.
- Cure, test and handover — cure window, electrical acceptance test, as-built drawings.

Schedule matters more here than on a thin-floor project. Each mortar layer needs to cure and be ground before the next goes down, so a 1,000 m² installation is planned in zones with defined access dates rather than as one continuous pour.
Thickness, service life and the cost of getting it wrong
The system is built at 8–12 mm. Thickness is confirmed on the specification sheet against the actual wheel loads, drop heights and chemical load of the area, not chosen from a catalog page.
| Система | Толщина | Quoted life | Duty |
|---|---|---|---|
| Coating (no reinforcement) | 0.3–1 mm | Varies | Foot traffic, light chemical contact |
| 3-cloth vinyl ester flooring | 3–5 mm | 5–8+ years | Chemical exposure, trolley traffic |
| Steel mesh heavy duty (this system) | 8–12 mm | 15+ лет | Forklifts, impact, abrasion, ESD control |
Quoted service life is 15+ years. The honest qualification: that assumes the substrate is structurally sound, the wheel loads were disclosed at enquiry stage, and the floor is not used as an anvil. Floors in this class usually fail from abuse — hot slag, dropped sharp loads, chemical spills left standing — rather than from material fatigue.
ACF-HX-SM-AS-SL is quoted from area, thickness, mesh specification, substrate condition, grounding layout and schedule. The cost gap between 8 mm and 12 mm is smaller than the cost of a failed 8 mm floor in a 12 mm duty, which is why we ask for wheel loads and drop heights before recommending a thickness.
Quotations are per square meter (sq ft) in FOB or CIF terms. Because the build is phased by bay, the minimum order is the smallest area that can be closed and cured as one pour, and lead time is given as a working-day range from sample approval.
Часто задаваемые вопросы
Is the whole build epoxy, or is it a vinyl ester floor?
The body is epoxy — primer, steel mesh mortar and glass flake leveling mortar — and the wearing surface is a vinyl ester self leveling topcoat. That combination is deliberate: epoxy gives the mechanical body and adhesion, vinyl ester gives the chemical and ESD performance at the surface where it is needed.
Can it be installed over an existing floor?
Over a sound, well-bonded resin floor in some cases, and over a prepared concrete slab in most. What cannot be done is building 8–12 mm of mesh-reinforced mortar over a delaminated coating or a slab with active moisture — the load will find the weak layer. We test adhesion and moisture before quoting a renovation.
What loads can it take?
That depends on the wheel type, the load per wheel, the slab thickness beneath and the sub-base. Those four inputs are what we ask for. A figure quoted without them would be meaningless, and a floor specified from a generic load table is how plants end up with cracked mortar under forklift aisles.
Does the anti static performance come from the topcoat only?
No. The vinyl ester topcoat is static-dissipative, the conductive putty spreads charge, and the copper grid carries it to earth. All three are needed; a dissipative topcoat over an insulative body with no earth path does not control charge.
Why projects specify Kaida Paint for heavy duty anti static flooring
Kaida Paint supplies the epoxy mortar body, the glass flake leveling mortar, the conductive putty and the vinyl ester topcoat as one system, with the mesh specification and the grounding layout issued alongside. Supplying the body and the topcoat from one source is what makes the intercoat window predictable on a build this thick — a mismatch there is invisible at handover and expensive two years later.
The technical file for each project records the wheel loads, the drop heights, the chemical list and the thickness actually installed, so the floor can be audited against the brief rather than against a brochure. Batch records and a material declaration ship with the material, and the method statement fixes substrate moisture, dew point and the cure interval between mortar layers.
Send the area, the wheel loads, the chemical list, the ESD target range and the schedule. We will return a thickness recommendation, an grounding layout and a quotation against those inputs.
-